Almost every building develops cracks at some point. Most cracks in walls and ceilings are harmless: the natural result of materials shrinking as they dry, or of plaster and paint responding to small daily changes in temperature and humidity. A minority are signs of something more serious, such as foundation movement, overloading or corrosion of reinforcement. The difficulty for owners is telling the two apart.
This guide explains, from the perspective of a practising structural engineer, how to read cracks: what their width, shape, location and behaviour tell you, which patterns are usually cosmetic, which deserve monitoring and which mean you should call an engineer without delay. It is general guidance, not a substitute for an inspection of your own building.
Why buildings crack
Concrete, masonry and plaster are strong in compression but weak in tension. When any part of them is pulled, bent or restrained from moving, a crack is the way the material relieves stress. The question is never whether a building will crack, but why a particular crack has formed and whether it is still moving.
The common causes fall into a few broad groups.
- Shrinkage. Concrete, cement render and plaster shrink as they dry and cure, producing fine cracks, often in the first year or two after construction or renovation.
- Thermal movement. Roof slabs, external walls and long elements expand and contract with temperature. Where movement is restrained, cracks form, often at junctions.
- Differing materials. Where a brick or block wall meets a concrete column or beam, the two materials move differently, and a crack often appears along the joint.
- Ground and foundation movement. Settlement, soft ground, changes in groundwater or nearby excavation can make parts of a building move relative to each other.
- Structural overload or deflection. Beams and slabs that deflect more than expected, because of additional loads or removed supports, can crack the walls and ceilings around them.
- Reinforcement corrosion. When steel in concrete rusts, it expands and splits the concrete around it, leading to cracking and eventually spalling.
Our guide to types of concrete cracks looks at these mechanisms in more detail.
Reading a crack: width, shape and location
Engineers look at several characteristics together. No single feature is conclusive, but the combination usually tells a clear story.
Width
A widely used reference for masonry walls is the damage classification in the UK Building Research Establishment’s Digest 251, which groups visible damage by typical crack width and ease of repair. Very broadly, cracks up to about 1 millimetre are regarded as very slight and are usually treated during normal redecoration; cracks up to about 5 millimetres are slight and easily filled; cracks of around 5 to 15 millimetres indicate moderate damage that may need some opening up and repair; and wider cracks indicate severe damage that warrants structural investigation. Width is only one indicator, and the classification describes damage rather than cause, but it is a useful starting framework.
Shape and direction
- Fine, random or map-like cracks in plaster or render are typically shrinkage and usually cosmetic.
- Straight vertical or horizontal cracks along wall-to-column or wall-to-beam junctions are often caused by differential movement between materials.
- Diagonal cracks, especially those running from the corners of door and window openings or in a stepped pattern through brickwork, can indicate differential settlement or movement and deserve closer attention.
- Tapered cracks, wider at one end than the other, suggest rotation or movement of one part of the structure relative to another.
- Cracks with rust staining, or cracks running along the line of a beam or slab soffit, may indicate corroding reinforcement.
Location
A crack in a non-structural partition is a different matter from a crack in a column, beam, structural wall or slab. Cracks in load-bearing elements always warrant more caution. If you are unsure which walls in your building are structural, check the approved plans or ask an engineer before assuming a crack is in a non-structural partition.
Ceiling cracks
Ceilings deserve their own mention because they are often where owners first notice problems. In plaster or board ceilings, fine cracks along joints are common and usually harmless. In concrete slabs, the picture is more varied.
Fine hairline cracks on a slab soffit are often shrinkage. Cracks accompanied by noticeable sagging, cracks that have widened over a short period, or cracks accompanied by water staining, rust marks or loose concrete fragments are different. In Singapore’s humid climate, water leaking through a slab from a bathroom or roof above can corrode reinforcement over time, and the first visible sign is often cracking followed by spalling concrete. That combination should be inspected rather than repainted.
Monitoring: is the crack moving?
A crack that formed years ago and has not changed is usually far less concerning than a crack that is growing. Establishing whether a crack is active is often the single most useful step an owner can take.
- Photograph the crack with a ruler or crack-width gauge alongside it, and note the date.
- Mark the ends of the crack lightly in pencil, with the date, so you can see if it extends.
- Repeat at regular intervals over several weeks or months, and note any changes in width or length.
- Watch for related signs: doors or windows that begin to stick, gaps opening at skirting or ceiling junctions, or floors becoming noticeably out of level.
Engineers may install tell-tale gauges or take precise measurements over time, especially where foundation movement is suspected. Our article on foundation settlement explains how movement is assessed and managed.
Cracks in walls: when to call a structural engineer
Use the following as a practical guide. Call an engineer promptly if any of these apply.
- Cracks are wider than a few millimetres, or are widening or lengthening over time.
- Diagonal or stepped cracks appear around openings, or tapered cracks suggest rotation.
- Cracks appear in columns, beams, structural walls or slabs, rather than only in plaster or partitions.
- Cracks are accompanied by rust staining, spalling or exposed reinforcement.
- Ceilings or floors are visibly sagging, or doors and windows have started to bind.
- Cracks appeared after nearby construction, excavation or piling, or after renovation works that removed or altered walls.
If cracking is sudden and severe, or accompanied by falling debris, move people away from the affected area and seek professional help immediately. In apartments and condominiums, inform the management corporation, since cracks in structural or common elements may be their responsibility. For HDB flats, contact your HDB Branch if you suspect a structural issue.
An engineer’s visit typically involves inspecting the cracks and their surroundings, considering the building’s history and any recent works, and, where necessary, recommending monitoring or further investigation. The findings are often summarised in a structural engineer’s report, which sets out the likely cause, the significance and the recommended repairs.
Repairing cracks properly
The right repair depends on the cause. Filling and repainting a cosmetic shrinkage crack is perfectly appropriate. Filling an active crack without dealing with its cause usually fails, because the crack simply reopens. Structural cracks may require resin injection, stitching, local strengthening or repair of corroded reinforcement, and in some cases treatment of the foundations.
The discipline is to diagnose first and repair second. If you have cracks that concern you and would like an independent, accountable assessment, our structural engineering consultancy can inspect and advise.
Frequently asked questions
Are cracks in walls normal?
Fine cracks in plaster and at junctions between different materials are very common and usually result from shrinkage or small thermal movements. They are typically cosmetic, but wider, growing or diagonal cracks, or cracks in structural elements, should be assessed by an engineer.
What size of wall crack is serious?
As a broad guide, cracks below about 1 millimetre are usually very slight, while cracks of around 5 millimetres or more indicate damage that warrants investigation. Width alone is not decisive; direction, location and whether the crack is growing matter just as much.
Are diagonal cracks worse than vertical cracks?
Diagonal and stepped cracks, especially from the corners of doors and windows, can indicate differential movement or settlement and deserve closer attention. Straight vertical cracks at wall-to-column junctions are more often caused by materials moving differently and are usually less concerning.
Should I worry about cracks in my ceiling?
Fine cracks along ceiling board joints or hairline shrinkage cracks in slabs are common. Cracks with sagging, water or rust staining, or loose concrete fragments should be inspected, since they may indicate leakage, corrosion of reinforcement or excessive deflection.
Can I just fill and paint over a crack?
For a stable, cosmetic crack, yes. For a crack that is moving or caused by a structural issue, filling it only hides the symptom and the crack will usually return, so the cause should be diagnosed and addressed first.
Why are there cracks in my new BTO flat?
Fine cracks in a new flat are usually shrinkage cracks, caused by concrete, plaster and skim coat drying out in the first year or two. They are typically hairline, random or along wall-to-beam junctions, and are generally cosmetic. Report them to HDB within the defects liability period, normally one year from key collection, so they can be assessed and rectified; wider, diagonal or growing cracks should be checked by an engineer.
Can nearby construction cause cracks in my walls?
Yes, piling, excavation, dewatering and heavy vibration nearby can cause ground movement that cracks walls, particularly in older buildings on soft ground. Large projects usually carry out a pre-construction condition survey of neighbouring buildings, which records existing cracks as a baseline. If new cracks appear, photograph them with dates and contact the developer or contractor, and ask for an independent engineer’s assessment where the damage is significant.
What is spalling concrete?
Spalling is when pieces of concrete break away from a slab, beam or column, usually because the steel reinforcement inside has corroded and expanded. It often starts as cracks with rust stains, then the cover concrete loosens and falls, exposing the bars. It is common under bathrooms and roofs in humid climates where water seeps through, and it should be repaired properly by removing loose concrete, treating the steel and reinstating with repair mortar.
What is crack injection and when is it used?
Crack injection is a repair in which low-viscosity epoxy or polyurethane resin is pumped into a crack under pressure to fill it. Epoxy can restore the bond across a dormant structural crack in concrete, while polyurethane is mainly used to stop water leaking through cracks. It only works once the cause has been identified and movement has stopped; injecting an active crack usually leads to it reopening.
Related reading
- BCA BP Submission: A Step-by-Step Guide to Building Plans
- Qualified Person Singapore: QPs and Accredited Checkers
- Certificate of Statutory Completion (CSC) Explained
- Temporary Occupation Permit Singapore: How TOP Works